Study on Thermal Decomposition of Intumescent Fire-Retardant Polypropylene by TG/Fourier Transform InfraredKey Laboratory of Rubber-Plastics for Ministry of Education, Qingdao University of Science and Technology, 53 Zheng Zhou Road Qingdao 266042, P.R. China
Key Laboratory of Rubber-Plastics for Ministry of Education, Qingdao University of Science and Technology, 53 Zheng Zhou Road Qingdao 266042, P.R. China, safetyqust{at}163.com
Key Laboratory of Rubber-Plastics for Ministry of Education, Qingdao University of Science and Technology, 53 Zheng Zhou Road Qingdao 266042, P.R. China The thermal decomposition processes of polypropylene formulations containing intumescent flame-retardant additives as well as the individual components in the composites have been studied using thermogravimetric analysis and real time Fourier transform infrared in both air and nitrogen atmospheres. The results show that the thermal decomposition processes of pure polypropylene (PP), polyamide, pentaerythritol, and intumecent flame-retarded PP (IFR-PP) composites in air are significantly different from that in nitrogen atmosphere. The existence of oxygen promotes the decomposition of the above materials. However, oxygen has little influence on the thermal decomposition of ammonium polyphosphate and zinc borate both in air and nitrogen atmospheres. All IFR-PP composites show an earlier onset of decomposition in comparison with pure PP both in nitrogen and air atmospheres. Accordingly, the initial release gases such as NH3 or H2O help to swell the melted PP polymer and improve the flame retardancy of IFR-PP composite. At temperature higher than 290°C in air and 440°C in nitrogen, the IFR-PP composites are more thermally stable than PP because of the incorporation of intumescent flame additives. The decomposition mechanisms of these materials are discussed based on the analysis of the results of TG/FTIR.
Key Words: thermal decomposition polypropylene intumescent fire-retardant TG FTIR.
This version was published on November
1, 2009 Journal of Thermoplastic Composite Materials, Vol. 22, No. 6,
681-701 (2009) |
||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||